Mechanisms and kinetics of organic matrix thermal oxidation

Chapitre d'ouvrage scientifique
Auteur
VERDU, Jacques
ccCOLIN, Xavier
86289 Laboratoire Procédés et Ingénierie en Mécanique et Matériaux [PIMM]

URI
http://hdl.handle.net/10985/18680
DOI
10.1007/978-1-4419-9308-3_8
Date
2012

Résumé

It is now well recognized that during thermal aging at moderate temperatures, for example, typically below the glass transition temperature, organic matrix composites perish mainly by matrix embrittlement resulting from its thermo-oxidation. The present chapter aims to briefly introduce this domain. The chapter consists of a brief history of polymer oxidation and description of mechanisms and kinetics. The radical character of oxidation processes; the main elementary steps: propagation, termination, initiation processes, and initial steps; structure-property relationships; the nature of oxidation products; and experimental methods for the study of oxidation mechanisms are also discussed. The standard kinetic scheme, case of oxygen excess and general shape of oxidation kinetic curves, the induction period, departure from Arrhenius law, and case of oxygen lack are described. Consequences of oxidation on matrix thermomechanical properties including chain scission and cross-linking physical approaches are presented.

Fichier(s) constituant cette publication

Nom:
PIMM_LTDPMC_2012_COLIN.pdf
Taille:
462.7Ko
Format:
PDF
Description:
Chapitres d'ouvrages scientifiques
Voir/Ouvrir

Cette publication figure dans le(s) laboratoire(s) suivant(s)

  • Laboratoire Procédés et Ingénierie en Mécanique et Matériaux (PIMM)

Documents liés

Visualiser des documents liés par titre, auteur, créateur et sujet.

  • Thermo-oxidation behaviour of composite materials at high temperatures: A review of research activities carried out within the COMEDI program 
    Article dans une revue avec comité de lecture
    LAFARIE, Marie Christine; GRANDIDIER, Jean Claude; OLIVIER, Loic; VERDU, Jacques; CINQUIN, Jacques; ccCOLIN, Xavier (Elsevier, 2010)
    The present paper presents a review of the main activities carried out within the context of the COMEDI research program, a joint collaboration involving three research teams focusing on the thermo-oxidation behaviour of ...
  • Diffusion-controlled radiochemical oxidation of bisphenol A polysulfone 
    Article dans une revue avec comité de lecture
    MONCHY-LEROY, Carole; AUDOUIN, Ludmila; VERDU, Jacques; ccCOLIN, Xavier; ccRICHAUD, Emmanuel (Wiley, 2011)
    The radiochemical degradation of bisphenol A polysulfone was investigated under a γ-ray dose rate of 24 kGy h-1 up to 30.7 MGy total absorbed dose at 60 °C using gel permeation chromatography, sol-gel analysis, glass ...
  • Radiochemical ageing of poly(ether ether ketone) 
    Article dans une revue avec comité de lecture
    FERREIRA, Paulo; AUDOUIN, Ludmila; VERDU, Jacques; MONCHY-LEROY, Carole; ccCOLIN, Xavier; ccRICHAUD, Emmanuel (Elsevier, 2010)
    Thin (60 μm) and thick (250 μm) samples of poly(ether ether ketone) were subjected to radiochemical ageing at 24 kGy h -1 dose rate for doses up to 30.7 MGy at 60 °C in air. FTIR spectrophotometry (hydroxyl and carbonyl ...
  • New Developments in the Field of Radiochemical Ageing of Aromatic Polymers 
    Chapitre d'ouvrage scientifique
    AUDOUIN, Ludmila; VERDU, Jacques; ccFAYOLLE, Bruno; ccCOLIN, Xavier; ccRICHAUD, Emmanuel (In Tech, 2012)
    Polymers having an aromatic backbone polymers have a high mechanical strength and a high modulus. Their aromaticity increases their resistance for use in relatively severe conditions especially in aerospace and nuclear ...
  • Effect of gamma irradiation on tensile properties of low molecular weight polyethylene samples 
    Article dans une revue avec comité de lecture
    MONCHY-LEROY, Carole; VERDU, Jacques; ccCOLIN, Xavier (Elsevier, 2011)
    Three high density polyethylene (PE) samples of different origins, with weight average molar masses ranging from 38 to 63kgmol-1 and displaying a semi-ductile behavior with strain at break εR values of the order of 100-140%, ...

Parcourir

Tout SAMLaboratoiresAuteursDates de publicationCampus/InstitutsCe LaboratoireAuteursDates de publicationCampus/Instituts

Lettre Diffuser la Science

Dernière lettreVoir plus

Statistiques de consultation

Publications les plus consultéesStatistiques par paysAuteurs les plus consultés

ÉCOLE NATIONALE SUPERIEURE D'ARTS ET METIERS

  • Contact
  • Mentions légales

ÉCOLE NATIONALE SUPERIEURE D'ARTS ET METIERS

  • Contact
  • Mentions légales