Progress in Materials ScienceAbstract
Liquid lead (Pb)- and lead–bismuth eutectic (LBE)-cooled fast neutron reactors (Gen-IV LFRs) are one of the most technologically mature fission reactor technologies, due to their inherent safety, high power density, and ability to burn nuclear waste. Accelerator-driven systems (ADS), in particular, promise to address the issues of long-lived radiotoxic nuclear waste, emerging uranium ore shortages, and the ever-increasing demand for energy. However, the conditional compatibility of conventional structural materials, such as steels, with liquid Pb and liquid LBE is still an important concern for the deployment of these advanced nuclear reactor systems, making the environmental degradation of candidate structural and fuel cladding steels the main impediment to the construction of Gen-IV LFRs, including ADS. This article presents a comprehensive review of the current understanding of environmental degradation of materials in contact with liquid Pb and liquid LBE, with a focus on the underlying mechanisms and the factors affecting liquid metal corrosion (LMC) and liquid metal embrittlement (LME), which are the two most important materials degradation effects. Moreover, this article addresses the most promising LMC and LME mitigation approaches, which aim to suppress their adverse influence on materials performance. An outlook of the needed future work in this field is also provided.
Files in this item
Related items
Showing items related by title, author, creator and subject.
-
Article dans une revue avec comité de lectureGONG, Xing; XIANG, Congying; AUGER, Thierry; CHEN, Jiajun; LIANG, Xiaocong; YU, Zhiyang; SHORT, Michael P; SONG, Min; YIN, Yuan (Elsevier BV, 2021)This paper reports a new liquid metal embrittlement (LME) system in which a dual-phase Al0.7CoCrFeNi (equimolar fraction) high-entropy alloy (HEA) is embrittled by lead-bismuth eutectic (LBE) at 350 and 500°C. At 350°C, ...
-
Article dans une revue avec comité de lectureGONG, Xing; AUGER, Thierry; ZHU, Wenjian; LEI, Huasheng; XIANG, Congying; YU, Zhiyang; SHORT, Michael; WANG, Pei; YIN, Yuan (Elsevier, 2021-12-23)After exposure to oxygen-poor (10^-13–10^-14 wt%) liquid lead-bismuth eutectic (LBE) at 500°C for 500 h, LBE penetrates more than one order of magnitude deeper in an FCC Al0.4CoCrFeNi high-entropy alloy (HEA) deco-rated ...
-
Article dans une revue avec comité de lectureWe report an ab-initio study of grain-boundary wetting (GBW) in three systems (Fe/Zn, Fe/Pb & Fe/Bi) on a Σ5(013)[100] tilt grain boundary. An energy-based approach is pursued and adapted to the study of liquid-metal/solid-metal ...
-
Article dans une revue avec comité de lecturePLANCHER, E.; TAJDARY, Pouya; AUGER, Thierry; CASTELNAU, Olivier; LOISNARD, Dominique; MARIJON, Jean-Baptiste; MAURICE, Claire; MICHEL, Vincent; ROBACH, Odile; STODOLNA, Julien (Springer Verlag (Germany), 2019)Synchrotron Laue microdiffraction and digital image correlation measurements were coupled to track the elastic strain field (or stress field) and the total strain field near a general grain boundary in a bent bicrystal. A ...
-
Article dans une revue avec comité de lectureBARKIA, Bassem; AUGER, Thierry; CABET, Céline; NICOLAS, Laetitia; ROBIN, Raphaël; RIVOLLIER, Matthieu; LORENTZ, Véronique; PERRIN, E. (Elsevier, 2018)In order to assess the susceptibility of candidate structural materials to Liquid Metal Embrittlement (LME), the fracture behavior of three grades of austenitic steels was investigated in oxygenated (200 wppm) liquid sodium ...