Direct keyhole laser welding of aluminum alloy AA5754 to titanium alloy Ti6Al4V
Article dans une revue avec comité de lecture
Date
2014Journal
Journal of Materials Processing TechnologyRésumé
The tensile strength of direct AA5754/Ti6Al4V joints performed by high speed Yb:YAG laser welding is found to be determined by morphology and phase content of dissimilar interface formed between contacting Al-rich and Ti-rich melted zones. Three types of contact interfaces were observed: (1) thin (<20 μm thick) interface composed mostly by TiAl and formed under 0.2 mm beam shift to Al side and linear energy of welding ≥37.5 kJ/m; (2) cracked interface (190–300 μm thick) composed by Al3Ti and other Al–Ti intermetallics and formed under beam shift at 0.2 mm to Ti side and linear energy ≥37.5 kJ/m; (3) malaxated interface composed of layers and isles of Ti3Al and TiAl forming in other tested conditions and favored by welding speed >10 m/min. Maximal linear tensile force (220 N/mm for 2 mm thick weld) can be attained when thin contact interface is formed. In this case, the fracture starts in intermetallics-rich zone but propagates mainly in Al-rich melted zone, when in other cases it occurs in brittle intermetallic layers.
Fichier(s) constituant cette publication
Cette publication figure dans le(s) laboratoire(s) suivant(s)
Documents liés
Visualiser des documents liés par titre, auteur, créateur et sujet.
-
Article dans une revue avec comité de lecturePEYRE, Patrice; BERTHE, Laurent; POUZET, Sébastien; SALLAMAND, Pierre; TOMASHCHUK, Iryna; DAL, Morgan (Elsevier, 2014)Laser-induced reactive wetting and brazing of T40 titanium with A5754 aluminum alloy with 1.5 mm thickness was carried out in lap-joint configuration, with or without the use of Al5Si filler wire. A 2.4 mm diameter laser ...
-
Article dans une revue avec comité de lecturePEYRE, Patrice; BERTHE, Laurent; POUZET, Sébastien; SALLAMAND, Pierre; TOMASHCHUK, Iryna; DAL, Morgan (Elsevier, 2014)Laser-induced reactive wetting and brazing of T40 titanium with A5754 aluminum alloy with 1.5 mm thickness was carried out in lap-joint configuration, with or without the use of Al5Si filler wire. A 2.4 mm diameter laser ...
-
Article dans une revue avec comité de lectureTOMASHCHUK, Iryna; SALLAMAND, Pierre; MÉASSON, A.; CICALA, E; DUBAND, M; PEYRE, Patrice (Elsevier, 2017)Laser assisted joining of AA5754 aluminum alloy to T40 titanium with use of Al-Si filler wires was carried out. Continuous Yb:YAG laser beam was shaped into double spot tandem and defocalized to cover larger interaction ...
-
Article dans une revue avec comité de lectureLHUISSIER, Pierre; HEBRARD, Louis; BATAILLON, Xavier; LAPOUGE, Pierre; COSTE, Frédéric; PEYRE, Patrice; BOLLER, Elodie; BLANDIN, Jean-Jacques; SALVO, Luc; MARTIN, Guilhem (AIP Publishing, 2022-08)We describe our miniature laser powder bed fusion (L-PBF) system for in situ synchrotron x-ray micro-computed tomography (XCT) at the European Synchrotron Radiation Facility. This replicator was designed to extend the ...
-
Article dans une revue avec comité de lectureCRENN, Marie-Joséphine; DUBOT, Pierre; MIMRAN, Elie; FROMENTIN, Olivier; LEBON, Nicolas; PEYRE, Patrice (MDPI AG, 2021-12)Electrochemically anodized (EA) surfaces promise enhanced biological properties and may be a solution to ensure a seal between peri-implant soft tissues and dental transmucosal components. However, the interaction between ...