Mechanical behavior study of plasma sprayed hydroxyapatite coatings onto Ti6Al4V substrates using scratch test
Article dans une revue avec comité de lecture
Date
2010Journal
Materials Science ForumRésumé
Mechanical behavior and fracture mechanisms of plasma sprayed hydroxyapatite coatings on Ti-6Al-4V substrate were assessed taking into consideration two variables: the coating thickness and the substrate roughness. The results show that the specimens having a substrate arithmetic average roughness parameter Ra = 2.29 μm is favorable with respect to Ra = 1.23 μm. For coating thickness above 105 μm, cracks can be observed in the coating/substrate interface and the higher critical load Pc2 (used generally in comparative evaluation of adherence) decreases. A 90 μm coating thickness sprayed on a substrate having an arithmetic average roughness parameter Ra equal to 2.29 μm seems to be the best compromise between microstructure, mechanical resistance (high critical loads and fairly good contact quality) and long term stability in the physiological medium (low dissolution rate) for an orthopedic application.
Fichier(s) constituant cette publication
Cette publication figure dans le(s) laboratoire(s) suivant(s)
Documents liés
Visualiser des documents liés par titre, auteur, créateur et sujet.
-
Article dans une revue avec comité de lectureBEHNAMGHADER, Aliasghar; SHARIFI, Davood; SOROORI, Sarang; BAGHERI, Narjes; TOULOUEI, Ranna; NEMATI, Roghieh; NAJJAR, Denis; IOST, Alain (2008)In this study, hydroxyapatite was coated on titanium substrates by plasma spraying process. A well-known porous and lamellar microstructure was found in the lateral and outer surface of coating. The phase composition was ...
-
Communication avec acteBEHNAMGHADER, Aliasghar; NAJJAR, Denis; IOST, Alain (societe française de métallurgie et de matériaux, 2006)L’objectif de cette étude est de caractériser le comportement fragile de l’hydroxyapatite (HAP) par évaluation de sa ténacité. Cette ténacité a été estimée pour des d’échantillons sous forme massive et pour des revêtements ...
-
Communication avec acteBEHNAMGHADER, Aliasghar; SHIRAZI, Reyhaneh Neghabat; IOST, Alain; NAJJAR, Denis (Trans Tech Publications, Switzerland, 2011)Surface degradation and cracking of dense hydroxyapatite were evaluated through Vickers micro indentation using indentation loads ranged from 25 gf to 2000 gf. Crack lengths, imprint diameters and the number of ...
-
Communication avec acteBEHNAMGHADER, Aliasghar; FARSADZADEH, B; NAJJAR, Denis; IOST, Alain (Springer, 2007)The extensive use of appropriate coatings to improve wear resistance, friction coefficient, electrical properties, corrosion resistance and biomedical application has stimulated a growing interest in their mechanical ...
-
Article dans une revue avec comité de lectureVAN GORP, Adrien; BIGERELLE, Maxence; GRELLIER, Alain; IOST, Alain; NAJJAR, Denis (Elsevier, 2007)This paper proposes a new multi-scale measurement approach performed to compare the surface roughness and the visual aspect of polished surfaces. In this investigation, five specimens of glass moulds presenting different ...