Generation and characterization of T40/A5754 interfaces with lasers
Article dans une revue avec comité de lecture
Auteur
Date
2014Journal
Journal of Materials Processing TechnologyRésumé
Laser-induced reactive wetting and brazing of T40 titanium with A5754 aluminum alloy with 1.5 mm thickness was carried out in lap-joint configuration, with or without the use of Al5Si filler wire. A 2.4 mm diameter laser spot was positioned on the aluminum side to provoke spreading and wetting of the lower titanium sheet, with relatively low scanning speeds (0.1 to 0.6 m/min). Process conditions did not play a very significant role on mechanical strengths, which were shown to reach 250-300 N/mm on a large range of laser power and scanning speeds. In all cases considered, the fracture during tensile testing occurred next to the TiAl3 interface, but in the aluminum fusion zone. In a second step, we have investigated the interfacial resistance with the LASAT bond strength tester, based upon the generation and propagation of laser-induced shock waves. This allowed us estimating a uniaxial bond strength of 0.68 GPa for the T40/A5754 interface under dynamic loading conditions.
Fichier(s) constituant cette publication
Cette publication figure dans le(s) laboratoire(s) suivant(s)
Documents liés
Visualiser des documents liés par titre, auteur, créateur et sujet.
-
Article dans une revue avec comité de lecturePEYRE, Patrice; BERTHE, Laurent; POUZET, Sébastien; SALLAMAND, Pierre; TOMASHCHUK, Iryna; DAL, Morgan (Elsevier, 2014)Laser-induced reactive wetting and brazing of T40 titanium with A5754 aluminum alloy with 1.5 mm thickness was carried out in lap-joint configuration, with or without the use of Al5Si filler wire. A 2.4 mm diameter laser ...
-
Article dans une revue avec comité de lectureTOMASHCHUK, Iryna; SALLAMAND, Pierre; CICALA, E; PEYRE, Patrice; GREVEY, D (Elsevier, 2014)The tensile strength of direct AA5754/Ti6Al4V joints performed by high speed Yb:YAG laser welding is found to be determined by morphology and phase content of dissimilar interface formed between contacting Al-rich and ...
-
Article dans une revue avec comité de lectureTOMASHCHUK, Iryna; SALLAMAND, Pierre; MÉASSON, A.; CICALA, E; DUBAND, M; PEYRE, Patrice (Elsevier, 2017)Laser assisted joining of AA5754 aluminum alloy to T40 titanium with use of Al-Si filler wires was carried out. Continuous Yb:YAG laser beam was shaped into double spot tandem and defocalized to cover larger interaction ...
-
Article dans une revue avec comité de lecturePEYRE, Patrice; POUZET, Sébastien; CASTELNAU, Olivier; DAL, Morgan (Laser Institute of America, 2017)The laser metal deposition (LMD) laser technique is a free-form metal deposition process, which allows generating near net-shape structures through the interaction of a powder stream and a laser beam. A simplified numerical ...
-
Article dans une revue avec comité de lectureMAYI, Yaasin; PEYRE, Patrice; BELLET, Michel; METTON, Charlotte; MORICONI, Clara; FABBRO, Rémy; DAL, Morgan (IOP Publishing, 2019)Although metal vaporisation has been observed in several laser processes such as drilling or welding, vapour plume expansion and its induced side effects are not fully understood. Especially, this phenomenon is garnering ...