Influence of the position and size of various deterministic defects on the high cycle fatigue resistance of a 316L steel manufactured by laser powder bed fusion
Article dans une revue avec comité de lecture
Date
2021Journal
International Journal of FatigueRésumé
Optimized 316L steel samples were manufactured using laser powder bed fusion and tested in high cycle fatigue at R = 0.1. They showed microstructural crack initiation and outstanding fatigue properties. Additional fatigue testings were then carried out on samples containing deterministic defects of various sizes and positions. All results summarized in a Kitagawa-Takahashi diagram show that the critical defect size is around 20 µm for surface defects and reach 380 µm for internal pores. Fracture surface analysis revealed that the large size gap between surface and internal fatigue crack initiation could be linked to the local gaseous environment in the pores.
Fichier(s) constituant cette publication
- Nom:
- PIMM_IJF_2021_ANDREAU.pdf
- Taille:
- 3.359Mo
- Format:
- Description:
- Article
- Fin d'embargo:
- 2021-08-01
Cette publication figure dans le(s) laboratoire(s) suivant(s)
Documents liés
Visualiser des documents liés par titre, auteur, créateur et sujet.
-
Texture control of 316L parts by modulation of the melt pool morphology in selective laser melting Article dans une revue avec comité de lectureANDREAU, Olivier; PEYRE, Patrice; PENOT, Jean-Daniel; DE TERRIS, Thibaut; DUPUY, Corinne; BAUDIN, Thierry; KOUTIRI, Imade; PESSARD, Etienne; SAINTIER, Nicolas (Elsevier, 2019)In this study, 316L parts were fabricated with the selective laser melting additive layer manufacturing process using unidirectional laser scan to control their texture. The melt pool shape, microstructure and texture of ...
-
Article dans une revue avec comité de lectureANDREAU, Olivier; PESSARD, Etienne; KOUTIRI, Imade; PENOT, Jean-Daniel; DUPUY, Corinne; SAINTIER, Nicolas; PEYRE, Patrice (Elsevier, 2019)Metal powder bed fusion techniques can be used to build parts with complex internal and external geometries.Process parameters are optimized in order to obtain parts with low surface roughness and porosity, while maintaining ...
-
Article dans une revue avec comité de lectureDE TERRIS, Thibaut; ANDREAU, Olivier; PEYRE, Patrice; ADAMSKI, Frédéric; GORNY, Cyril; DUPUY, Corinne; KOUTIRI, Imade (Elsevier, 2019)The systematic occurrence of porosities inside selective laser melted (SLM) parts is a well-known phenomenon. In order to improve the density of SLM parts, it is important not only to assess the physical origin of the ...
-
Article dans une revue avec comité de lecturePEYRE, Patrice; AMLOU, Ouafae; DE TERRIS, Thibaut; KOUTIRI, Imade; PESSARD, Etienne (Elsevier, 2018)This paper is dedicated to understanding fatigue crack initiation for an Inconel 625 manufactured by SLM, using a hatching + contour procedure. In the first part of the paper, an optimum set of parameters was found to ...
-
Article dans une revue sans comité de lectureGUNENTHIRAM, V; PEYRE, Patrice; SCHNEIDER, Matthieu; COSTE, Frédéric; FABBRO, Rémy; DAL, Morgan; KOUTIRI, Imade (Elsevier, 2018)The experimental analysis of spatter formation was carried out on an instrumented SLM set-up allowing the quantification of spatter ejections and possible correlation with melt-pool behavior. Considering nearly similar SLM ...