Soumissions récentes

  • QUEIROZ, D. P.R.; FRAÏSSE, Frédéric; FAYOLLE, Bruno; KUNTZ, Matthias; VERDU, Jacques (Elsevier Ltd., 2010)
    The degradation of an epoxy-amine network exposed to gamma irradiation in oxygen atmosphere has been studied by using a variety of analytical methods, including infrared spectroscopy (FTIR), differential scanning calorimetry ...
  • BIJAR, Ahmad; ROHAN, Pierre-Yves; PERRIER, Pascal; PAYAN, Yohan (Springer Science and Business Media LLC, 2015-11-17)
    Generation of subject-specific 3D finite element (FE) models requires the processing of numerous medical images in order to precisely extract geometrical information about subject-specific anatomy. This processing remains ...
  • FRAME, Jamie; ROHAN, Pierre-Yves; CORTE, Laurent; ALLENA, Rachele (2017-07-03)
    Introduction Improper osseointegration of implants leading to poor mechanical anchoring or embrittlement of neighboring bone is a major concern in orthopedic surgery [1?]. This integration is known to depend on the complex ...
  • PRADERE, Christophe; CAUMES, Jean-Pascal; BENKHEMIS, S.; PERNOT, Jean-Philippe; PALOMO, Elena; DILHAIRE, S.; BATSALE, Jean-Christophe (AIP Publishing, 2014-06)
    GigaHertz (GHz) thermoreflectance technique is developed to measure the transient temperature of metal and semiconductor materials located behind an opaque surface. The principle is based on the synchronous detection, using ...
  • GRAEFF, Eliot; MARANZANA, Nicolas; AOUSSAT, Améziane (Taylor & Francis, 2019-07-23)
    Engineering design, as the science framing the practice of design through the elaboration of tools and processes, is constantly evolving towards new innovative strategies. To thrive in their extremely competitive environment, ...
  • RICHAUD, Emmanuel; FERREIRA, Paulo; AUDOUIN, Ludmila; COLIN, Xavier; VERDU, Jacques; MONCHY-LEROY, Carole (Elsevier Ltd., 2010)
    Thin (60 μm) and thick (250 μm) samples of poly(ether ether ketone) were subjected to radiochemical ageing at 24 kGy h -1 dose rate for doses up to 30.7 MGy at 60 °C in air. FTIR spectrophotometry (hydroxyl and carbonyl ...
  • SARRABI, Salah; COLIN, Xavier; TCHARKHTCHI, Abbas (Wiley Periodicals, Inc., 2010)
    The main drawback of rotational molding is a long stay (several dozens of minutes) of polymer in melt state at high temperature in atmospheric air. To prevent any significant polymer thermal degradation, it is necessary ...